Non-shrink repair composition on small-grained gritter of poured type containing polymer fibre. It is used with a destruction depth from 15 to 40 mm on horizontal lower stratums and surfaces with a gradient of not more than 4% (per 1 meter).
SURFACE PREPARATION
It is applied on a concrete lower stratum from the surface of which previously it is necessary to remove: cement slurry, loose coating, the remains of old coatings, paints, etc. To perform these works, the use of a milling machine is recommended. Before the mortar mix applying to the surface to be repaired, it is necessary to eliminate active leakages using the rapid-hardening, expanding GLIMS®ГидроПломба repair composition. If the reinforcement is open and has instances of corrosion, it must be cleaned of rust and dirt, and then treated with a corrosion-preventive compound. Before the repair mortar applying, the surface of the lower stratum must be supplied with clean water up to a full saturation level. Thickness of application in one layer is from 15 to 40 mm, if the depth of the repaired area exceeds 40 mm, it is necessary to fasten the metal mesh to the lower stratum leaving a space between the mesh and the surface of at least 10 mm. If the lower stratum is not strong enough, after the reinforcement mounting it is necessary to treat the repaired area with Glims®PrimeГрунт. When material applying and hardening the temperature of the lower stratum and the environment should not be lower than +5 ° C. For more information refer to the coating laying flow diagram.
MORTAR PREPARATION
Pour the package contents into a reservoir with clean water at a rate of 0.12-0.14 l of water per 1 kg of dry mix (3-3,5 l per bag of 25 kg) and mix thoroughly with a mixer machine to even consistency. Keep the mortar for 2-3 minutes and then mix it once more.
TECHNOLOGY OF WORK EXECUTION
The ready for use mortar mix should be applied using special equipment (for example, for air placing) or manually. The mortar mix pouring is performed continuously - from one side of the defective area to the other. This is necessary to prevent air entering and void formation in the mortar mix. Mortar mix pouring from two opposite sides is not allowed. When using the material for thicknesses up to 300 mm, it is necessary to add gravel chippings graded of 5-10 mm from solid rocks (granite, ragstone, gabbro, toadstone) in an amount up to 40% of the mortar weight. Add gravel chippings to the prepared mortar mix and mix to even consistency. The mixture containing is laid manually. To ensure optimal applied mortar mix solidification conditions it is necessary to protect its top layer from water evaporation using a polymer film or to moisten the surface with finely sprayed cold water for 24 hours (48 hours in hot and windy weather). Solidification time and subsequent finishing to a greater extent are dependent on environmental conditions. Operation temperature range – from -50 to +70 ° С. While working it is necessary to observe the norms of SNiP and industrial hygiene. The material is environmentally friendly in use and operation.
CONSUMPTION:
2,1 kg/m2 with a layer thickness of 1 mm.
TRANSPORTATION AND STORAGE
During transportation and storage, bags with dry mortar should be protected from damage and soaking. The storage period is 12 months. Complies with GOST R 56378-2015 (class R4)